Nanocyl EPOCYL™ NC E128-02 Master Batch Liquid Bisphenol-A Resin for non-Solvent Based Formulation Purposes

Category Polymer , Thermoset , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Nanocyl
Trade Name EPOCYL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nanocyl EPOCYL™ NC E128-02 Master Batch Liquid Bisphenol-A Resin for non-Solvent Based Formulation Purposes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EPOCYL™ NC E128-02 is a Mater Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl. It is specifically developed to enhance electrical conductivity of epoxy-based formulations. Special features include easy integration and great flexibility in design of new multifunctional materials. Dilution factor has to be calculated accordingly to the desired level of conductivity.ApplicationsElectrostatic discharge (ESD) coatings, linings (tanks, rollers, ...) and compositesConductive primersResistive inksAdhesivesBenefitsLimited impact on base resin mechanical and thermo-mechanical propertiesEase of formulationOther information available upon request to NanocylCuring agents EPOCYL™ NCE128-02 based formulations can be cured or cross-linked with different types of curing agents which could be decided accordingly to the desired processing conditions and the properties of the final composite like any conventional Bis-A based formulations.Properties measured on cast films.
Physical Properties Metric English Comments
Specific Gravity 1.15 - 1.20 g/cc
1.15 - 1.20 g/cc
Viscosity 350000 - 450000 cP

@Temperature 25.0 °C
350000 - 450000 cP

@Temperature 77.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 100 ohm-cm
100 ohm-cm
80 parts per 100 of NC E128-02 in the final compound
200 ohm-cm
200 ohm-cm
53 parts per 100 of NC E128-02 in the final compound
2000 ohm-cm
2000 ohm-cm
26 parts per 100 of NC E128-02 in the final compound
10000 ohm-cm
10000 ohm-cm
13 parts per 100 of NC E128-02 in the final compound
Descriptive Properties Value Comments
Aspect Paste, black (Master Batch)
Epoxy Equivalent 190.5 -198 g/eq
Epoxy Value 5.05 - 5.25 eq/kg
Storage Temperature 5°C - 40°C