Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 350000 - 450000 cP @Temperature 25.0 °C |
350000 - 450000 cP @Temperature 77.0 °F |
|
Nanocyl EPOCYL™ NC E128-02 Master Batch Liquid Bisphenol-A Resin for non-Solvent Based Formulation Purposes EPOCYL™ NC E128-02 is a Mater Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl. It is specifically developed to enh.. |
|||
Viscosity | 350000 - 450000 cP @Temperature 25.0 °C |
350000 - 450000 cP @Temperature 77.0 °F |
|
Nanocyl EPOCYL™ NC R128-02 Master Batch Liquid Bisphenol-A Resin for Hot-Melt Formulation Purposes: Dilution Factor 6 EPOCYL™ NC R128-02 is a Master Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl, with a suggested dilution factor of.. |
|||
Viscosity | 25000 - 450000 cP | 25000 - 450000 cP | Average value: 242000 cP Grade Count:6 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Viscosity | 150000 - 450000 cP | 150000 - 450000 cP | |
Lord Adhesives 22 Mix-In Red Accelerator for 200, 400, 500 Series Lord Adhesives 22 Mix-In Red Accelerator for 200, 400, 500 SeriesLord Accelerator 22 is a red mix-in accelerator for use with all Lord Acrylic Adhesives. Use at 2:1 and 4:1 ratios for Lord 200, 400,.. |
|||
Viscosity | 150000 - 450000 cP | 150000 - 450000 cP | |
Lord Adhesives 19 Mix-In Accelerator for 200, 400, 500 Series Lord Adhesives 19 Mix-In Accelerator for 200, 400, 500 SeriesLord Accelerator 19 Mix-in accelerator. Use at 2:1 or 4:1 ratio for Lord 200, 400 and 500 Series Acrylic Adhesives. Well-suited for meter.. |
|||
Viscosity | 150000 - 450000 cP | 150000 - 450000 cP | |
Lord Adhesives 19B Mix-In Black Accelerator for 200, 400, 500 Series Lord Adhesives 19B Mix-In Black Accelerator for 200, 400, 500 SeriesLord Accelerator 19 Black Mix-in accelerator. Use at 2:1 or 4:1 ratio for Lord 200, 400 and 500 Series Acrylic Adhesives. Well-sui.. |
|||
Viscosity | 250000 - 450000 cP | 250000 - 450000 cP | Dynamic |
Dow Corning 9546 Silicone Elastomer Blend A mixture of high molecular weight silicone elastomers (dimethicone crosspolymer) in cyclopentasiloxane and a high molecular weight linear silicone polymer for use in skincare, suncare, shower gel, .. |