Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning XIAMETER® PMCPMEM-1171 Emulsion

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name XIAMETER®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning XIAMETER® PMCPMEM-1171 Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is chemically equivalent to DOW CORNING® 2-1171 EMULSION. Non-ionic, 50% emulsion of polydimethylsiloxane.Information provided by Dow Corning
Physical Properties Metric English Comments
pH 7.0
7.0
Processing Properties Metric English Comments
Shelf Life 15.0 Month
15.0 Month
Descriptive Properties Value Comments
Active Content (%) 50
Color White
Hydrophobic Yes
Non-Ionic Yes
Users viewing this material also viewed the following: