Northstar Polymers PNA-216 Curing Agent

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Liquid
Manufacturer Northstar Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Northstar Polymers PNA-216 Curing Agent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Northstar Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.003 g/cc
1.003 g/cc
Viscosity 1300 cP

@Temperature 22.2 °C
1300 cP

@Temperature 72.0 °F
Descriptive Properties Value Comments
Equivalent Weight 2074