Material Notes:
PERMABOND® ET515 is a 1:1 mixable epoxy adhesive. ET515 is a semi-flexible toughened adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and composites. It’s a relatively fast curing epoxy; reaching handling strength in 15 minutes. It is ideal for bonding different materials where differential thermal expansion is anticipated. Features & Benefits: Adhesion to a wide variety of substrates Full cure at room temperature Easy to apply High shear and peel strength Good impact strength Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ET515A, Epoxy Resin
1.14 g/cc
1.14 g/cc
ET515B, Polyamine Hardener
Viscosity 19000 cP

@Temperature 25.0 °C
19000 cP

@Temperature 77.0 °F
ET515B, Polyamine Hardener
20000 cP

@Temperature 25.0 °C
20000 cP

@Temperature 77.0 °F
ET515A, Epoxy Resin
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
Elongation at Break 30 %
30 %
Adhesive Bond Strength 3.00 - 5.00 MPa
435 - 725 psi
FRP Glass/Polyester, Shear; ASTM D1002
4.00 - 6.00 MPa
580 - 870 psi
FRP Glass/Epoxy, Shear; ASTM D1002
4.00 - 6.00 MPa
580 - 870 psi
Carbon Fiber, Shear; ASTM D1002
8.00 - 12.0 MPa
1160 - 1740 psi
Mild steel, Shear; ASTM D1002
Peel Strength 2.40 - 3.20 kN/m
13.7 - 18.3 pli
ISO 4578
Thermal Properties Metric English Comments
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 80.0 °C
176 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 40.0 °C
104 °F
Processing Properties Metric English Comments
Cure Time 15.0 - 30.0 min
0.250 - 0.500 hour
handling time
4320 min
72.0 hour
full cure
Pot Life 10.0 - 15.0 min

@Temperature 20.0 °C
10.0 - 15.0 min

@Temperature 68.0 °F
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Amber for Polyamine Hardener
Colorless for Epoxy Resin
Maximum Gap Fill (mm) 2
Strength Retention 10% at 150°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 100°C
Relative to 0°C
93% at 50°C
Relative to 0°C
Copyright © lookpolymers.com All Rights Reserved