NOVA Chemicals Sclair® FP120-D Octene LLDPE Film Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer NOVA Chemicals
Trade Name Sclair®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® FP120-D Octene LLDPE Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Food packaging, freezer film, lamination and sealant filmInformation provided by Nova Chemicals
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Thickness 25.0 microns
0.984 mil
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.0 MPa
1450 psi
ASTM D882
Film Tensile Strength at Yield, TD 10.0 MPa
1450 psi
ASTM D882
Film Elongation at Yield, MD 480 %
480 %
ASTM D638
Film Elongation at Yield, TD 670 %
670 %
ASTM D882
Puncture Energy 0.900 J
0.664 ft-lb
Low Friction Puncture
Elmendorf Tear Strength MD 420 g
420 g
ASTM D1922
Elmendorf Tear Strength TD 605 g
605 g
ASTM D1922
Dart Drop Test 270 g
0.595 lb
ASTM D1709/A
Film Tensile Strength at Break, MD 48.0 MPa
6960 psi
ASTM D882
Film Tensile Strength at Break, TD 32.0 MPa
4640 psi
ASTM D882
1% Secant Modulus, MD 174.95 MPa
25375 psi
ASTM D882
1% Secant Modulus, TD 194.95 MPa
28275 psi
ASTM D882
Optical Properties Metric English Comments
Haze 10 %
10 %
ASTM D1003
Gloss 59 %
59 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 210 - 230 °C
410 - 446 °F