Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ISO 527-3 |
Polimeri Europa Clearflex® FG B3 Very Low Density Polyethylene Clearflex FG B3 is a linear low density polyethylene, with antioxidants, slip and antiblocking agents, suitable for blown film technology. The product is characterized by a very low density and a h.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ISO 527-3 |
Polimeri Europa Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene Flexirene FF 25 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FF 25 is characterized by a high elongational viscosi.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ISO 527-3 |
Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Flexirene FH 56 A are characte.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
NOVA Chemicals Novapol® TD-9055-E Hexene LMDPE Film Resin Excellent stiffness and glossApplications: Diaper back sheet, BlendingAdditives: High temperature AOFilm properties are typical of cast film extruded at 280°C.Information provided by NOVA Chemicals.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-0119-D Hexene LLDPE Film Resin Film Properties. Features: Exceptional toughness, high strength with thin films.Applications: Thin films, premium trash bags, ice bags.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-0119-F Hexene LLDPE Film Resin Film Properties. Features: High strength and toughness, low gel count.Applications: Stretch wrap, blend resin.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-0338-E Hexene LMDPE Film Resin Excellent stiffness and glossApplications: Diaper back sheet, BlendingAdditives: High temperature AOFilm properties are typical of film extruded at 280°C.Information provided by NOVA Chemicals. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin Film Properties. Features: Excellent stiffness, excellent puncture, high strength and toughness.Applications: Industrial packaging, overwrap, narrow die gap extrusion.Data provided by the manufactu.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y826-CP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness, intended for narrow die gaps, high strength and toughness.Applications: Industrial bags, industrial packaging.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
NOVA Chemicals Sclair® FP120-D Octene LLDPE Film Resin Applications: Food packaging, freezer film, lamination and sealant filmInformation provided by Nova Chemicals |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ISO 527-3 |
Polimeri Europa Clearflex® FG B0 Very Low Density Polyethylene Clearflex FG B0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FG B0 are highly transparent, have good sealing properties, even.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene CopolymerCharacteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applicationsApplications:Bakery Films, Coextr.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Strength and toughness, good sealing properties, suitable for narrow die gaps.Applications: Industrial packaging, heavy duty sacks.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
NOVA Chemicals Sclair® 11U4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, easy processability.Applications: Bread bags, HDPE bottle sleeves, specialty blending.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
Chevron Phillips HiD® 9640 HDPE Blown Film Resin
(discontinued **) Copolymerization Enhances Film Toughness, Unique Combination of Density and Melt Index, Excellent Strength Properties as well as Good Heat Seal, Lower Density Imparts a Softer Feel and Lesser Tenden.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y826-D Hexene LLDPE Film Resin Film Properties. Features: High strength and toughness, excellent puncture resistance, good stiffness and machinability.Applications: Premium trash bags, bags-on-roll.Data provided by the manufactu.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
Iran Petrochemical (PCC) 09X02 Linear Low Density Polyethylene 09X02 is a high performance LLDPE (HP-LLDPE) cast film grade combines ease of processing with low gels and good film strength. Its excellent stretchability makes this grade particularly suited for s.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882-02 |
Ipiranga Petrochem LB 0316 LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
Iran Petrochemical (PCC) 235F7 Linear Low Density Polyethylene 235F7 is a LLDPE blown film grade designed for general purpose film application. This resin is particularly suited for blending with LDPE, giving better strength and downgauging possibility.Informat.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ISO 1184 |
SIDPEC EGYPTENE® LL 0209 AA LLDPE Film Applications:Heavy duty sacksAgricultural films and linersProduce bags, stretch filmFilm properties were measured on 15 micron film extruded at a blow up ratio of 2:1.Information provided by Interch.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ISO 1184 |
SIDPEC EGYPTENE® LL 0209 KJ LLDPE Film Applications:Refuse sacksProduce bags, carrier bagsFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ISO 527-3 |
Total LLDPE LL 1820 H Linear Low Density Polyethylene - Blown Film LL 1820 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 H can be processed at high o.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
Total Lotrene® Q2018C Linear Low Density Polyethylene, Blown Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | |
Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade DOWLEX® 2077 Polyethylene resin is a fully formulated linear low density polyethylene resin designed for use in food packaging applications. This blown film resin is designed to run on narrow die-g.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
Braskem LF 0720/20 AF LLDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Heavy duty bags; "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
Braskem LF 0720/21 AF LLDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); high clarity films; "liners"; general purpose. Information provided by Braskem |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
Chevron Phillips 6335B LLDPE Cast/Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, Medium Slip Version of 6335Characteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applications, Lo.. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-0119-FP Hexene LLDPE Film Resin
(discontinued **) Film Properties. Features: High strength and toughness, low gel count, intended for narrow die gaps.Applications: Stretch wrap, blend resin.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, TD | 32.0 MPa | 4640 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y826-BP Hexene LLDPE Film Resin
(discontinued **) Film Properties. Features: Good stiffness and machinability, intended for narrow die gaps, high strength and toughness.Applications: Grocery sacks, boutique bags, frozen food packaging.Data provide.. |