Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T LFH 238 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LFH 238 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion. It contains slip and antiblocking a.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Riblene® FC 26 Low Density Polyethylene - Blown Film Extrusion Riblene FC 26 is a high molecular weight low density polyethylene (LDPE), with added antiblocking agent, suitable for blown film extrusion. Riblene FC 26 is characterized by a high melt strength le.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 22 Low Density Polyethylene - Blown Film Extrusion Riblene FF 22 is a high molecular weight low density polyethylene (LDPE), with added slip agent, suitable for blown film extrusion. Riblene FF 22 is characterized by a good melt strength leading to.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 24 Low Density Polyethylene - Blown Film Extrusion Riblene FF 24 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 24 is characterized by a good melt s.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 34 Low Density Polyethylene - Blown Film Extrusion Riblene FF 34 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 34 is characterized by a good melt s.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Riblene® FL 20 Low Density Polyethylene - Blown Film Extrusion Riblene FL 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FL 20 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin Film Properties. Features: Free flowing granules, toughness and strength, ease of extrusion.Applications: Blending, concentrates.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0219-A LDPE Foam Resin Features: Good heat sealing latitudeModerate toughnessEasy processability Applications: Industrial packagingLinersBlends with LLDPEFoam ArticlesInformation provided by Nova Chemicals |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE Puncture value is 60 J/mm. Additive Package: Antiblock.Applications: industrial liners, heavy duty packaging.Film properties are typical of 25 µm blown film extruded at a blow-up ratio of 2.5:1, b.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-0119-F Hexene LLDPE Film Resin Film Properties. Features: High strength and toughness, low gel count.Applications: Stretch wrap, blend resin.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y822-BP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, exceptional toughness.Applications: Industrial packaging, high strength liners.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Sclair® FP120-D Octene LLDPE Film Resin Applications: Food packaging, freezer film, lamination and sealant filmInformation provided by Nova Chemicals |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D 882 |
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 75 Micron Film FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T CMH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CMH 108 show e.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
SABIC HP0722N Low Density Polyethylene for Blown Film Product Description: HP0722N is a Low Density Polyethylene grade suitable for producing medium duty films and contains no slip or antiblock additives. It yields good toughness and optical properti.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Strength and toughness, good sealing properties, suitable for narrow die gaps.Applications: Industrial packaging, heavy duty sacks.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Sclair® 12J1 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity.Applications: Overwrap, lamination.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
Iran Petrochemical (PCC) Arak 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0218-AB LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Good heat sealing latitude, Moderate toughness, E.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D 882 |
NOVA Chemicals Novapol® PF-0218-E Butene Copolymer LLDPE Film Resin PF-0218-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® PF-0218-F Butene LLDPE Film Resin Toughness and strength, Ease of extrusionApplications: Cast films, BlendingAdditives: Process stabilizerFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depende.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y822-CP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, exceptional toughness, suitable for narrow die gaps.Applications: Heavy duty sacks, high strength packaging.Data provided by the manufac.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 1184 |
SIDPEC EGYPTENE® LL 0209 AA LLDPE Film Applications:Heavy duty sacksAgricultural films and linersProduce bags, stretch filmFilm properties were measured on 15 micron film extruded at a blow up ratio of 2:1.Information provided by Interch.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 1184 |
SIDPEC EGYPTENE® LL 0209 KJ LLDPE Film Applications:Refuse sacksProduce bags, carrier bagsFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 1184 |
SIDPEC EGYPTENE® LL 0220 AA LLDPE Film Applications:Light and medium duty filmStretch filmFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 1184 |
SIDPEC EGYPTENE® LL 0220 KJ LLDPE Film Applications: Light and medium duty film.Film properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor of Sidi Ke.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | 2 in per min; ASTM D882 |
Chevron Phillips MarFlex® D139 m-LLDPE Linear Low Density Polyethylene Low Density PolyethyleneCustomer Benefits: Possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved processability (bubble stability, down-.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Sclair® 11G1 LLDPE Film Resin
(discontinued **) Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionAdditives: Process stabilizer, Polymer process aidFilm properties are typical of blown film.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0218-AF LDPE Extrusion Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |