Physical Properties Metric English Comments
Melt Flow 5.4 g/10 min

@Load 21.6 kg,
Temperature 190 °C
5.4 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
SABIC FI0644 Bimodal High Density Polyethylene for Blown Film
Product Description: FI0644 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Melt Flow 5.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Network Polymers Softflex® 5000
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Melt Flow 5.4 - 9.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
5.4 - 9.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 6250D (506H4) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 5.4 g/10 min

@Load 21.6 kg,
Temperature 190 °C
5.4 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) EX 6HT HM 9455 HT High Density Polyethylene
EX 6HT is a high density polyethylene with 1-Butene as co monomer. It has good toughness, low gel level, good tear strength, high tenacity.Applications: film extrusion, blending partner, refuse ba..
Melt Flow 5.4 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.4 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Diamond Polymers ASA S124 ASA Weatherable Polymers Injection Molding Grade, Medium Modulus
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 5.4 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.4 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ASA S210
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ModulusInformation provided by Diamond Polymers, Inc.
Melt Flow 5.4 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.4 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ASA S210B
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ModulusInformation provided by Diamond Polymers, Inc.
Melt Flow 5.4 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.4 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Diamond Polymers ASA S-210E ASA Weatherable Polymers Extrusion Molding Grade, Medium Modulus
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.