Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.30 - 0.50 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.30 - 0.50 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6250D (506H4) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.30 - 0.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.30 - 0.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PP 8332C (EPD60R) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Melt Flow | 0.20 - 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR Plus High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.20 - 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR Plus T10 High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.20 - 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR Plus T15 High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.20 - 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR White F High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.20 - 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR White F60 High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |