Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MRC Polymers SATRANâ„¢ 805 ABS Terpolymer, Impact Modified

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer MRC Polymers
Trade Name SATRAN™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MRC Polymers SATRANâ„¢ 805 ABS Terpolymer, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MRC Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D 792
Water Absorption 0.40 %
0.40 %
ASTM D 570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D 955
Melt Flow 2.0 - 5.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.0 - 5.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.0 MPa
5510 psi
ASTM D 638
Flexural Strength 59.0 MPa
8560 psi
ASTM D 790
Flexural Modulus 2.069 GPa
300.1 ksi
ASTM D 790
Izod Impact, Notched 0.910 J/cm

@Temperature -20.0 °C
1.70 ft-lb/in

@Temperature -4.00 °F
ASTM D 256
2.08 J/cm

@Temperature 23.0 °C
3.90 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
189 °F
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
171 °F
ASTM D 648