Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS (Asia Pacific) LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP AI001XXH ABS LNP* Lubricomp* AI001XXH is a compound based on ABS containing 2% Silicone. Characteristics of this grade are: Healthcare and Internally Lubricated. |
|||
Tensile Strength, Yield | 38.0 - 137 MPa | 5510 - 19800 psi | Average value: 91.6 MPa Grade Count:23 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | |
Ineos ABS Lustran® QE 1094 AS, Injection Grade
(discontinued **) Injection molding grade, super high impact.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638 |
Ineos H20Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO R527 |
Fainplast Compounds RK 335/1 Rigid PVC, Extrusion Lead Free Profiles |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM-D638 |
Ineos ABS Lustran® 720 ABS, Molding Grade Lustran® ABS 720 resin is a black, virgin injection molding grade of ABS (acrylonitrile butadiene styrene). It is supplied as salt-and-pepper pellets with color concentrate 901802 black. Designed.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638-02 |
Ipiranga Petrochem PH 3515 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527 |
SABIC Innovative Plastics LNP Lubriloy Z2000 PPE+PS LNP* Lubriloy* Z2000 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP fo.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON SX90398 PA 12 LNP STAT-KON* SX90398 is a compound based on Nylon 12 resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY A3000TXB ABS LNP* STAT-LOY* A3000TXB is a compound based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives and Bioassessed to ISO 10993... |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | 50mm/min; ISO 527 |
Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP M7002XXH PP LNP* THERMOCOMP* M7002XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additives. Designed for touch surfaces in healthcare applications. Added features include:.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638 |
Wico Plast Wicoran 47 ABS, Impact Resistant ApplicationsInjection moldingExtrusionCharacteristics:Impact resistantAll information provided by Wico Plast, Warenhandelsges. mbH |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-530KF15 A5M Polymer Alloy Main Characteristics: High elongation; High impact strength; Stress resistantApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInformation provided by Zed.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527 |
A. Schulman FORMION™ FI 232H 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232H is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, high stiffness and exceptional impact.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527-1/-2 |
Unitika ET2025 PA6, Conditioned High-impact nylonInformation provided by Unitika Ltd. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | parallel; ISO 527-3 |
Covestro Desmopan® 445 Polyurethane injection molding gradegrease and oil-resistantgood heat resistancelow compression setApplicationAutomotive engineeringInjection molded engineering partsPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527-2 |
Denka MALECCA K-095 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638 |
Aclo Accucomp ABS ABS804L High Impact Grade |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638 |
Teknor Apex Sinpolene FRF2074 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Flame Retardant Uses: Appliance Components; Housings Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638 |
Teknor Apex Sinpolene TPP1030 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 30% Filler by Weight Uses: Automotive Applications; Housings Forms: Pellets Processing Method: Injection .. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultraform® N2650 Z6 POM + PUR Description: Elastomer-modified injection molding grade for applications requiring highest impact strength together with low stiffness.Information provided by BASF |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527 |
A. Schulman FORMION™ FI 232H 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232H is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, high stiffness and exceptional impact.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy FXW710SK ASA/SAN (Europe-Africa-Middle East) GELOY FXW710SK is an ASA/SAN injection moulding grade. It is suitable for those applications that require sparkle colour effects.This data was supplied by SABIC-IP for the Europe-Africa-Middle East .. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638 |
Braskem H 501 HC Bioriented Film Polypropylene Applications: High stiffness; barrier films for conversionInformation provided by Braskem |