Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 38.0 MPa | 5510 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG29 ABS Super high impact ABS. Good low temperature toughness. High gloss. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY XTWE265 ASA (Asia Pacific) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS (Asia Pacific) LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Europe-Africa-Middle East) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638 |
Ineos Nova 2504 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Good balance of flow, strength and heat resistance, USP Class VI Applications: Consumer electronics, HousewaresExposure to gamma radiation in the 2.02-6.06 megarad range has no .. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO R527 |
Fainplast Compounds RH 306/W Rigid PVC, Antishock Extrusion Antishock profiles |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638 |
Flint Hills P4C5B-181B Polypropylene Homopolymer Features: Nucleated and Antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: Closures and cutleryInformation Provided by Flint Hills Resour.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638 |
Ineos Nova 3100 General Purpose Crystal Polystyrene Good balance of flow and set-up properties, Good crack resistanceApplications: Single service cutlery, Single service drinkware, Consumer electronic packagingExposure to gamma radiation in the 2.02-.. |
|||
Tensile Strength, Yield | 38.0 MPa @Strain 0.200 %, Temperature 1093 °C |
5510 psi @Strain 0.200 %, Temperature 1999 °F |
|
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP MX06404 PP LNP LUBRICOMP* MX06404 is a compound based on Polypropylene resin containing 20% Glass Fiber and 15% PTFE. Added features of this material include: Heat Stabilized, Low Extractable, Wear Resistant... |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRILOY Z2000 PPO LNP* LUBRILOY* Z2000 is a compound based on PPO resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON SX90398 PA 12 LNP STAT-KON* SX90398 is a compound based on Nylon 12 resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS LNP STAT-LOY* A3000 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Asia Pacific) LNP STAT-LOY A3000 is a compound based on Acrylonitrile butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistatic. Also known as: STAT-LOY A |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Europe-Africa-Middle East) LNP* Stat-loy* A3000 is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: Antistat. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS (Asia Pacific) LNP* Stat-loy* AF306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Antistat. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | parallel; ISO 527-3 |
Covestro Desmopan® 445 Polyurethane injection molding gradegrease and oil-resistantgood heat resistancelow compression setApplicationAutomotive engineeringInjection molded engineering partsPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | 50 mm/min; ISO 527 |
Chi Mei Polylac® PA-737 ABS - High Flow High flow, medium impact |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527-2 |
Denka MALECCA K-090 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO 527-2 |
Denka MALECCA K-100 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638 |
Aclo Accucomp ABS ABS804L High Impact Grade |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | 50 mm/min; ISO 527-2 |
BASF Ultraform® N2650 Z6 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grade for applications requiring the highest impact strength together with low stiffness.Information provided by BASF |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638 |
Teknor Apex Sinpolene FRF2074 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Flame Retardant Uses: Appliance Components; Housings Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | Conditioned 15 days at 23°C - 50% RH; ISO 527 |
Arkema Group Rilsamid® PA 12 AMNO MED Nylon 12 Rilsamid® AMNO MED is a thermoplastic polyamide 12. This grade dedicated to injection offers the highest quality and it is specifically designed to meet the stringent requirements of the medical ap.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | |
Fainplast Compounds RE 130 Rigid PVC, Extrusion Pipes and profiles |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | |
Fainplast Compounds RE 224 Rigid PVC, Extrusion Various profiles |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ISO R527 |
Fainplast Compounds RE 430 Rigid PVC, Extrusion Electric channels |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | 50 mm/min |
Arkema Group Rilsan® BESHV Nylon 11, Blow Molding Grade (Conditioned) Designation ISO 1874-PA11,E,24-010Rigid grade for extrusion blow molding. Available color: natural. Additive free.Very good impact strength. Well adapted melt strength. High chemical resistance.Food.. |
|||
Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638 |
Ineos H07D-00 Polypropylene Homopolymer Grade H07D-00 is a polypropylene homopolymer for cast film applications that require slip and antiblock additives. This resin meets the requirements of the Food and Drug Administration as specified .. |