Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Purell® PE1840H Low Density Polyethylene, Blown Film, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Blow Molding Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Purell®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Purell® PE1840H Low Density Polyethylene, Blown Film, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Purell PE 1840 H is a low density polyethylene with good flexibility and is delivered in pellet form. It is designed for small blow molding but can also be used in film applications and injection molding. It can be used for medical devices and packaging of pharmaceuticals.Regulatory Status: Purell PE 1840 H meets the requirements of the Food and Drug Administration, Code of Federal Regulations, 21CFR Section 177.1520. This regulation allows the use of this olefin polymer in "articles or components of articles intended for use in contact with food." Contact your Equistar sales representative for more information regarding the suitability of specific products for specific applications. Specific recommendations for processing Purell PE 1840 H can only be made when the processing conditions, equipment, and end use are known. For further suggestions, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 50.8 microns
2.00 mil
Melt Flow 1.5 g/10 min
1.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 47
47
ASTM D2240
Tensile Strength at Break 12.2 MPa
1770 psi
ASTM D638
Tensile Strength, Yield 10.8 MPa
1560 psi
ASTM D638
Elongation at Break 670 %
670 %
ASTM D638
Tensile Modulus 0.254 GPa
36.9 ksi
1% Secant; ASTM D638
Flexural Modulus 0.241 GPa
35.0 ksi
1% Secant; ASTM D790
Dart Drop 2.36 g/micron
60.0 g/mil
ASTM D1709
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Optical Properties Metric English Comments
Haze <= 11 %
<= 11 %
ASTM D1003
Gloss >= 20 %
>= 20 %
20°; ASTM D2457
75 %
75 %
Gardner, 60°; ASTM D523
Processing Properties Metric English Comments
Melt Temperature 180 °C
356 °F
Blow-up Ratio (BUR) 2.0
2.0