Polymer Property : Flexural Modulus = 0.241 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.241 GPa
35.0 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE D 4210 BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Flexural Modulus 0.241 GPa
35.0 ksi
Tangent; ASTM D790
RheTech Products E206-01 Linear Low Density Polyethylene, Black
Applications: Flexible componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 0.241 GPa
35.0 ksi
Tangent; ASTM D790
RheTech Products FT1100-689UV Thermoplastic Polyolefin, UV Stabilized, Light Natural Beige
Applications: Pillar plugsAirbag doorsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
S&E Specialty Polymers GPE2001F-ROHS PVC
Application: GPE2001F-ROHS is flame retardant polyethylene compound designed for wire and cable applications. GPE2001F-ROHS complies with RoHS requirements. GPE2001F-ROHS is suitable for 75°C cont..
Flexural Modulus 0.241 - 3.85 GPa
35.0 - 558 ksi
Average value: 2.17 GPa Grade Count:76
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Flexural Modulus 0.241 GPa
35.0 ksi
1% Secant; ASTM D790
Multibase Multi-Flex® A 9702 MR TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Flexural Modulus 0.241 GPa
35.0 ksi
1% Secant; ASTM D790
Multibase Multi-Flex® D 3804 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P..
Flexural Modulus 0.241 GPa
35.0 ksi
tangent; ASTM D790
Spartech EP5240 Calcium Carbonate Filled Homopolymer
Provides the highest level of stiffness and heat resistance of filled olefins. Calcium Carbonate filled grades offer an excellent balance of stiffness and impact resistance. Typical applications inc..
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
Teknor Apex Monprene® MP-1956A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
Flexural Modulus 0.241 GPa
35.0 ksi
secant-transverse direction; ASTM D882
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Flexural Modulus 0.241 GPa
35.0 ksi
secant-transverse direction; ASTM D882
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
Flexural Modulus 0.241 GPa
35.0 ksi
secant-transverse direction; ASTM D882
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Flexural Modulus 0.241 GPa
35.0 ksi
secant-transverse direction; ASTM D882
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Flexural Modulus 0.241 GPa
35.0 ksi
secant-transverse direction; ASTM D882
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
Flexural Modulus 0.241 GPa
35.0 ksi
secant-transverse direction; ASTM D882
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Flexural Modulus 0.241 GPa
35.0 ksi
ISO 178
DSM Fibre Intermediates Nyrim® 4000 (Conditioned)
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
Dow SPECTRIM™ 35-S Reaction Moldable Polymer
SPECTRIM™ 35-S reaction moldable polymer is a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology developed by the Dow Chemical Company.Information p..
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
Techmer ES HiFill® TPU 0445 A
Availability: North AmericaForms: PelletsFeatures: High Density and High Specific GravityInformation provided by TP Composites, Inc.
Copyright © lookpolymers.com All Rights Reserved