Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 12.2 MPa @Temperature 23.0 °C |
1770 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne OnFlex™ HFFR 361-0190 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 361-0190 is a non-halogen flame retardant material designed for injection molding applications. New Product. Commercial specifications have not been established. - UL 94 HB compliantPu.. |
|||
Tensile Strength at Break | 12.2 MPa | 1770 psi | ASTM D638 |
ExxonMobil Escorene® LD 725.21 Molding, extrusion, compounding and adhesive resin
(discontinued **) Escorene Ultra LD 722.21 is 18 wt% vinyl acetate copolymer suitable for molding, extrusion, compounding and hot melt adhesive applications.Information provided by ExxonMobil Chemical |
|||
Tensile Strength at Break | 12.2 MPa | 1770 psi | ASTM D638 |
LyondellBasell Purell® PE1840H Low Density Polyethylene, Blown Film, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding Purell PE 1840 H is a low density polyethylene with good flexibility and is delivered in pellet form. It is designed for small blow molding but can also be used in film applications and injection mo.. |