Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 10.8 MPa | 1560 psi | ASTM D638 |
LyondellBasell Purell® PE1840H Low Density Polyethylene, Blown Film, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding Purell PE 1840 H is a low density polyethylene with good flexibility and is delivered in pellet form. It is designed for small blow molding but can also be used in film applications and injection mo.. |
|||
Tensile Strength, Yield | 10.8 MPa | 1560 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3300-85 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 10.8 MPa | 1560 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SPF 9020 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Stiffness Uses: Gaskets; Profiles; Seals Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |