Lucite International Diakon® TD510 Toughened Acrylic Compound

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Impact Modified, Molded
Manufacturer Lucite International
Trade Name Diakon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Diakon® TD510 Toughened Acrylic Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by injection molding or extrusion.Information provided by Lucite International
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183
Water Absorption 0.30 %
0.30 %
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
Melt Flow 3.5 g/10 min
3.5 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 88
88
ISO 2039-2
Tensile Strength 65.0 MPa
9430 psi
ISO 527
Elongation at Break 10 %
10 %
ISO 527
Flexural Modulus 2.90 GPa
421 ksi
ISO 178
Izod Impact, Notched (ISO) 2.40 kJ/m²
1.14 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.210 J/cm²
0.999 ft-lb/in²
ISO 179/1eA
2.20 J/cm²
10.5 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
ASTM E831
Vicat Softening Point 103 °C
217 °F
ISO 306B
112 °C
234 °F
ISO 306A
Heat Distortion Temperature 93.0 °C
199 °F
ISO 75A
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
IEC 695-2-1
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ISO 489
Haze 2.0 %
2.0 %
ASTM D1003
Transmission, Visible 91 %
91 %
ASTM D1003