Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525 |
Plaskolite Optix® CA-924 Impact Modified Acrylic Resin Injection Molding Grade Pellets. Good impact strength. |
|||
Vicat Softening Point | 112 °C | 233 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 927 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525 |
Plaskolite West Optix® CA-924 Impact Modified Acrylic Resin Injection Molding Grade Pellets. Good impact strength. |
|||
Vicat Softening Point | 112 °C | 233 °F | ASTM D-1525 |
Plaskolite West Optix® CP - 927 G High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Vicat Softening Point | 112 °C @Load 1.00 kg |
234 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Flexirene® MR 50 A Linear Low Density Polyethylene Flexirene MR 50 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 A are characterized by optimum rigidity... |
|||
Vicat Softening Point | 112 °C @Load 1.00 kg |
234 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Flexirene® MR 56 A Linear Low Density Polyethylene Flexirene MR 56 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 A are characterized by optimum rigidity... |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® BPL1000 PC (Europe-Africa-Middle East) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Vicat Softening Point | 112 °C | 233 °F | ASTM D-1525 |
Plaskolite Optix® CP - 924 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate A, ASTM D1525 |
Plaskolite West Optix® CA-927 G Clear Impact Modified Acrylic Resin Impact modified acrylic resin, injection molding gradeApplications: An impact-modified acrylic resin designed for medical or food uses. This resin offers impact strengths up to seven times of gener.. |
|||
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525 |
NOVA Chemicals Sclair® 8406 UV8D, 8406G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer. |
|||
Vicat Softening Point | 112 °C | 234 °F | 50°C/h 50N (from DAM) |
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (Conditioned) Key Features:Contains FillerSuitable processing methods:Injection molding |
|||
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525 |
Micropol Microlin ML25 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics PREVEX VGAX PPE+PS Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 180F HDT. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific) Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific) Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow. |
|||
Vicat Softening Point | 112 °C | 234 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® NH-1037 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 112 °C | 234 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® NH-1037 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 112 °C | 234 °F | (50 °C/h / 50N) - B/50; ISO 306 |
Styrolution Terluran® HH-112 ABS Terluran HH-112 is an injection molding grade of ABS with very high heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Noryl PX0003 PPE+HIPS PX0003 resin is a modified PPE+PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gr.. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Noryl PX0003 PPE+HIPS PX0003 resin is a modified PPE+PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gr.. |
|||
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525, ISO 306 |
DuPont™ Fusabond® P353 Polymer Modifier DuPont Fusabond® P353 is a chemically modified polypropylene. Uses: Automotive Applications Plastics Modification Polymer Modifier Applications: Coupling agent Long glass fiber filled PP compoun.. |
|||
Vicat Softening Point | 112 °C | 234 °F | ExxonMobil Method |
ExxonMobil Pax-Plus™ 3208 Blown Film Resin Pax-Plus 3208 is a rubber modified high density polyethylene film resin offering good physical properties with ease of processing. It exhibits toughness, stress crack resistance and low WVTR.Inform.. |
|||
Vicat Softening Point | 112 °C | 234 °F | |
Dow DOWLEX™ 2071 Linear Low Density Polyethylene DOWLEX® 2071 Polyethylene resin is a linear low density polyethylene resin specifically designed for the manufacture of high strength, thin gauge films for use in applications such as grocery sacks.. |
|||
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525 |
Proto3000 PC-ABS Fused Deposition Modeling Polymer Description: PC-ABS (polycarbonate-ABS) is one of the most widely used industrial thermoplastics. PC-ABS offers the most desirable properties of both materials - the superior strength and heat resis.. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |