Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.210 - 1.00 J/cm²

@Temperature -30.0 - 30.0 °C
0.999 - 4.76 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 0.582 J/cm² Grade Count:31
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Charpy Impact, Notched 0.210 - 7.50 J/cm²
0.999 - 35.7 ft-lb/in²
Average value: 0.984 J/cm² Grade Count:155
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Charpy Impact, Notched 0.210 J/cm²
0.999 ft-lb/in²
ISO 179/1eA
Solvay Specialty Polymers Amodel® A-1230 L Polyphthalamide (PPA)  (discontinued **)
Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten..
Charpy Impact, Notched 0.210 J/cm²
0.999 ft-lb/in²
ASTM D256
Plenco 4759 Phenolic, Granular, Injection Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and possesses good electrical properties. It is used in appli..
Charpy Impact, Notched 0.210 J/cm²
0.999 ft-lb/in²
ASTM D256
Plenco 7300 Phenolic, Nodular, Injection Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file..
Charpy Impact, Notched 0.210 J/cm²
0.999 ft-lb/in²
ASTM D256
Plenco 7527 Phenolic, Nodular, Injection Molded  (discontinued **)
Single-Stage Phenolic. PLENCO 07527 is a flock cotton and mineral filled resole phenolic molding compound.Information supplied by Plenco
Charpy Impact, Notched 0.210 J/cm²
0.999 ft-lb/in²
J/cm; ASTM D256
Plenco Valite 759 Novolac Phenolic, Granular, Injection Molded  (discontinued **)
This Valite product has been replaced by Plenco 4759. Data provided by Plenco.VALITE 759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and p..
Charpy Impact, Notched 0.210 J/cm²
0.999 ft-lb/in²
ISO 179/1eA
Lucite International Diakon® ST15G6 Toughened Acrylic Polymer
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b..
Charpy Impact, Notched 0.210 J/cm²
0.999 ft-lb/in²
ISO 179/1eA
Lucite International Diakon® TD510 Toughened Acrylic Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by..
Charpy Impact, Notched 0.210 J/cm²

@Temperature 23.0 °C
0.999 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Borealis PS65C40 Polypropylene Compound, Mineral Filled
PS65C40 is a 40% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and..
Charpy Impact, Notched 0.210 J/cm²

@Temperature 23.0 °C
0.999 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Ensinger TECASINT 4201 SD Polyimide, Black, Carbon Fiber (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Charpy Impact, Notched 0.210 J/cm²
0.999 ft-lb/in²
Biomer P209 PHB Biodegradable Polymer
PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P..
Charpy Impact, Notched 0.210 - 5.40 J/cm²
0.999 - 25.7 ft-lb/in²
Average value: 1.36 J/cm² Grade Count:26
Overview of materials for Acrylic, Impact Modified, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values ..
Copyright © lookpolymers.com All Rights Reserved