Lotte Chemical Titan TITANEX® HF0961 High density polyethylene Hexene-1 resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Lotte Chemical Titan Holding Sdn. Bhd. (Former Titan Chemicals)
Trade Name TITANEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANEX® HF0961 High density polyethylene Hexene-1 resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HF0961 is a pelleted high molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners notion and millinery bags.Advantages: High extrusion rate with high film strength and rigidity, excellent drawdown for high quality thin film.Information provided by Titan Chemicals
Physical Properties Metric English Comments
Base Resin Density 0.950 g/cc
0.0343 lb/in³
ASTM D1505
Thickness 17.0 microns
0.669 mil
extruded at 4:1 BUR
Base Resin Melt Index 0.10 g/10 min
0.10 g/10 min
I<sub>2</sub>; ASTM D1238
11 g/10 min
11 g/10 min
I<sub>21</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 250 %
250 %
ASTM D882
Film Elongation at Break, TD 700 %
700 %
ASTM D882
Elmendorf Tear Strength, MD 0.400 g/micron
10.2 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 3.00 g/micron
76.2 g/mil
ASTM D1922
Dart Drop 8.00 g/micron
203 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 58.8 MPa
8530 psi
ASTM D882
Film Tensile Strength at Break, TD 44.1 MPa
6400 psi
ASTM D882
1% Secant Modulus, MD 1176.8 MPa
170680 psi
ASTM D882
1% Secant Modulus, TD 1280 MPa
185000 psi
ASTM D882
Processing Properties Metric English Comments
Melt Temperature 180 - 240 °C
356 - 464 °F
Blow-up Ratio (BUR) 4.0
4.0