Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 58.8 MPa | 8530 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® HF0961 High density polyethylene Hexene-1 resin HF0961 is a pelleted high molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners notion and millinery bags.Advantag.. |
|||
Film Tensile Strength at Break, MD | 58.8 MPa | 8530 psi | ASTM D882 |
Chevron Phillips Dynex™ D605C3 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |