Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 3.00 g/micron | 76.2 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANEX® HF0961 High density polyethylene Hexene-1 resin HF0961 is a pelleted high molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners notion and millinery bags.Advantag.. |
|||
Elmendorf Tear Strength, TD | 3.00 g/micron | 76.2 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANZEX® HF7000 High density polyethylene HF7000 is a high density polyethylene resin for tubular film extrusion. HF7000 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1.. |