Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Melt Index | 0.10 g/10 min | 0.10 g/10 min | I<sub>2</sub> |
Lotte Chemical Titan TITANEX® HB0972 High density polyethylene Hexene-1 resin HF0972 is a pelleted high density polyethylene Hexene-1 resin for blow molding.Applications: Large size shipping containers and drums, household and industrial chemical containers, toiletries and c.. |
|||
Base Resin Melt Index | 0.10 g/10 min | 0.10 g/10 min | I<sub>2</sub>; ASTM D1238 |
Lotte Chemical Titan TITANEX® HF0961 High density polyethylene Hexene-1 resin HF0961 is a pelleted high molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners notion and millinery bags.Advantag.. |