Base Resin Melt Index 0.10 g/10 min
0.10 g/10 min
I<sub>2</sub>
Lotte Chemical Titan TITANEX® HB0972 High density polyethylene Hexene-1 resin
HF0972 is a pelleted high density polyethylene Hexene-1 resin for blow molding.Applications: Large size shipping containers and drums, household and industrial chemical containers, toiletries and c..
Base Resin Melt Index 0.10 g/10 min
0.10 g/10 min
I<sub>2</sub>; ASTM D1238
Lotte Chemical Titan TITANEX® HF0961 High density polyethylene Hexene-1 resin
HF0961 is a pelleted high molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners notion and millinery bags.Advantag..