Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 1280 MPa | 186000 psi | ASTM D822 |
LyondellBasell Alathon® L5906 High Density Polyethylene ApplicationsALATHON XL 5906 is a high molecular weight high density polyethylene homopolymer with a broad bimodal molecular weight distribution. This resin exhibits excellent stiffness, very high t.. |
|||
1% Secant Modulus, TD | 1280 MPa | 185000 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® HF0961 High density polyethylene Hexene-1 resin HF0961 is a pelleted high molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners notion and millinery bags.Advantag.. |
|||
1% Secant Modulus, TD | 1280 MPa | 186000 psi | 1 in/min; ASTM D882 |
Total HDPE HL 535 High Density Polyethylene, Film Resin Polyethylene: Medium molecular weight, high density film resinCharacteristics:High stiffnessGood heat resistanceExcellent bubble stabilityGood compatibility with LDPE and LLDPEApplications:Release .. |