Lehmann & Voss LUVOCOM® 1105-8279 PEEK, with CNT

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1105-8279 PEEK, with CNT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated electricity.Chemical and hydrolysis resistance parts, non flammable.Highly dimensionally stable at elevated temperatures.Parts for electric and electronic industry.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
23°C/24h
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
Mechanical Properties Metric English Comments
Tensile Stress 100 MPa
14500 psi
Elongation at Yield 5.6 %
5.6 %
6.8 %
6.8 %
flexural
Modulus of Elasticity 5.00 GPa
725 ksi
Flexural Strength 160 MPa
23200 psi
Flexural Modulus 4.00 GPa
580 ksi
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
flatwise; ISO 179 1fU
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
260 °C
500 °F
short term
Flammability, UL94 V-0
V-0
not recognized by UL
Electrical Properties Metric English Comments
Surface Resistance <= 1.00e+6 ohm
<= 1.00e+6 ohm
Insulation Resistance <= 1.00e+6 ohm
<= 1.00e+6 ohm
Processing Properties Metric English Comments
Processing Temperature 390 °C
734 °F
mass temp
Nozzle Temperature 360 - 380 °C
680 - 716 °F
Zone 1 360 - 370 °C
680 - 698 °F
Zone 2 380 - 390 °C
716 - 734 °F
Zone 3 390 - 400 °C
734 - 752 °F
Mold Temperature 170 - 200 °C
338 - 392 °F
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
150 °C

@Time 10800 - 21600 sec
302 °F

@Time 3.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color black