Material Notes:
Description: This mullite bonded, corundum brick combines a very good thermal shock resistance with a low creep as well as with resistance against a large variety of slags. (after 50 hours at 1650°C at a load of 0.2 MPa during the last 20 hours the creep is approximately 0.3%).Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 3.15 g/cc
0.114 lb/in³
Apparent
Porosity 16 %
16 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 100 MPa
14500 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 2.70 W/m-K

@Temperature 1100 °C
18.7 BTU-in/hr-ft²-°F

@Temperature 2010 °F
2.80 W/m-K

@Temperature 650 °C
19.4 BTU-in/hr-ft²-°F

@Temperature 1200 °F
3.10 W/m-K

@Temperature 100 °C
21.5 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 1760 °C
3200 °F
Deformation under load - t<sub>a</sub>
1760 °C
3200 °F
Component Elements Properties Metric English Comments
Al2O3 94 %
94 %
Fe2O3 <= 0.20 %
<= 0.20 %
SiO2 5.0 %
5.0 %
Descriptive Properties Value Comments
Segercone 41
Thermal Shock Resistance 30 cycles
DIN 51068