Material Notes:
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubrication and abrasion resistance, excellent chemical resistance, wide usage temperature, good impact absorbing characteristicsInformation provided by US distributor, API-Kolon.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
DIN 53479; ASTM D792
Water Absorption 0.70 %
0.70 %
DIN 53475; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
DIN 53505; ASTM D785
Tensile Strength, Ultimate 63.7 MPa
9250 psi
DIN 53455; ASTM D638
Elongation at Break 10 %
10 %
DIN 53455; ASTM D638
Flexural Yield Strength 118 MPa
17100 psi
DIN 53455; ASTM D790
Flexural Modulus 3.92 GPa
569 ksi
DIN 53452; ASTM D790
Izod Impact, Notched 0.686 J/cm
1.29 ft-lb/in
DIN 53453; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature 20.0 °C
22.2 µin/in-°F

@Temperature 68.0 °F
DIN 53752; ASTM D696
Melting Point 220 °C
428 °F
DIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
DIN 53461; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
DIN 53461; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149/DIN 53481
Arc Resistance 136 sec
136 sec
ASTM D495