TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is carried out by the use of various peroxides including dicumyl peroxide (DCP) or 2,5-dimethyl-2,5-bis (t-butylperoxy) hexane (DBPH).FormulationMillathane 5004100Stearic Acid0.25N330 (HAF) Black20Di-Cup 40C3All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Tensile Strength, Yield 28.8 MPa
4170 psi
Elongation at Yield 560 %
560 %
100% Modulus 0.00276 GPa
0.400 ksi
200% Modulus 0.00669 GPa
0.970 ksi
300% Modulus 0.0126 GPa
1.83 ksi
Tear Strength 99.8 kN/m
569 pli
ASTM Die C
Processing Properties Metric English Comments
Cure Time 2.00 min

@Temperature 204 °C
0.0333 hour

@Temperature 400 °F