Lucite International Elvacite ® 4080 Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Elvacite ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvacite ® 4080 Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvacite® 4080 is a medium molecular weight methyl methacrylate copolymer. It is a relatively flexible acrylic resin useful for improving the recoatability and intercoat adhesion of UV wood finishes, based on epoxy or urethane acrylates.Information provided by Lucite International
Physical Properties Metric English Comments
Particle Size 100 - 250 µm
100 - 250 µm
Brookfield Viscosity 1350 cP

@Temperature 23.0 °C
1350 cP

@Temperature 73.4 °F
30% wt in HDDA
Molecular Weight 33000 g/mol
33000 g/mol
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 75.0 °C
167 °F
Chemical Properties Metric English Comments
Total Acid Number 0.00
0.00