Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kleerdex Kydex® 150 Acrylic/PVC Thermoplastic Sheet  (discontinued **)

Category Polymer , Thermoplastic , Acrylic (PMMA) , Vinyl (PVC) , PVC/Acrylic Alloy
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kleerdex Kydex® 150 Acrylic/PVC Thermoplastic Sheet  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Class I/A rated thermoplastic sheetApplications: Interior ductwork and chutes, laboratory hoods, shower/tub shrouds, acoustical applications, decorative ceilings, abuse resistant surfacing for counters, exhibits, portions, doorsFeatures: Kydex 150 is more resistant to a wider range of concentrated chemicals than any other thermoplastic. Its superior chemical resistance allow for excellent cleanability because stronger clearing agents can be sued with no discoloration or surface damage to the material. It is not available for field applied wallcovering applications. Flammability Properties: Flame Spread at 25 minutes. Fire Door at 20 minutes (ASTM E152).Fabrication: Kydex 150 has good formability and extensibility and is extremely easy to work with once formed. All secondary operations, such as sawing, shearing, punching, and brake forming are possible with Kydex 150 sheet.Data provided by the Kleerdex Company.Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ASTM D785
Tensile Strength, Ultimate 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 160 %
160 %
Modulus of Elasticity 2.31 GPa
335 ksi
Flexural Yield Strength 64.0 MPa
9280 psi
ASTM D790
Izod Impact, Notched 9.53 J/cm

@Temperature 23.0 °C
17.9 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Taber Abrasion, mg/1000 Cycles 0.038
0.038
ASTM D1044
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
annealed; ASTM D648