Mechanical Properties Metric English Comments
Izod Impact, Notched 9.53 J/cm

@Temperature 23.0 °C
17.9 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Kleerdex Kydex® 101 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Thermoplastic sheet for signageApplications: Sign applications, radomes, other applications where a weatherable color over a white substrate is desirableFeatures: Kydex 101 is more rigid than most o..
Izod Impact, Notched 9.53 J/cm

@Temperature 23.0 °C
17.9 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Kleerdex Kydex® 120 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
USDA approved thermoplastic sheetApplications: High impact resistant wallcovering, push plates and kick plates, equipment housings, splash and safety guardsFeatures: Kydex 120 meets class I/A fire c..
Izod Impact, Notched 9.53 J/cm

@Temperature 23.0 °C
17.9 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Kleerdex Kydex® 150 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Class I/A rated thermoplastic sheetApplications: Interior ductwork and chutes, laboratory hoods, shower/tub shrouds, acoustical applications, decorative ceilings, abuse resistant surfacing for count..