Material Notes:
This TPO product is suitable for outdoor applications with good low temperature properties and UV resistance in applications such as ridge vents.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792-91
Melt Flow 9.0 g/10 min
9.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 20.7 MPa
3000 psi
ASTM D638-95
Elongation at Break 1200 %
1200 %
ASTM D638-95
Flexural Modulus 0.6207 GPa
90.03 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched NB
NB
ASTM D-256-93a
Gardner Impact 10.7 J
7.89 ft-lb
ASTM D5420-93