Polymer Property : Modulus of Elasticity = 2.31 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.31 GPa
335 ksi
Kleerdex Kydex® 120 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
USDA approved thermoplastic sheetApplications: High impact resistant wallcovering, push plates and kick plates, equipment housings, splash and safety guardsFeatures: Kydex 120 meets class I/A fire c..
Modulus of Elasticity 2.31 GPa
335 ksi
Kleerdex Kydex® 150 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Class I/A rated thermoplastic sheetApplications: Interior ductwork and chutes, laboratory hoods, shower/tub shrouds, acoustical applications, decorative ceilings, abuse resistant surfacing for count..