Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elastocon TPE Technologies Elastocon® STK55PA Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Elastocon TPE Technologies
Trade Name Elastocon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastocon TPE Technologies Elastocon® STK55PA Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elastocon® STK55PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK55PA is well suited for consumer goods and industrial applications requiring non-slip/soft touch ergonomics, sound and vibration dampening, improved impact resistance, and U.V. stability. Elastocon® STK55PA can be overmolded to nylon.Information provided by Elastocon® TPE Technologies
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 53
53
ASTM D2240
Tensile Strength, Yield 4.56 MPa
661 psi
ASTM D412
Elongation at Break 333 %
333 %
ASTM D412
100% Modulus 0.00270 GPa
0.392 ksi
ASTM D412
Processing Properties Metric English Comments
Rear Barrel Temperature 250 - 260 °C
482 - 500 °F
Front Barrel Temperature 265 - 277 °C
509 - 531 °F
Nozzle Temperature 277 - 285 °C
531 - 545 °F
Mold Temperature 82.0 - 104 °C
180 - 219 °F
Back Pressure 0.345 - 0.689 MPa
50.0 - 99.9 psi
Descriptive Properties Value Comments
Injection Velocity (mm/sec) Fast
Users viewing this material also viewed the following: