Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mearthane Durethaneâ„¢ F DF-245A Closed Cell Foam Polyurethane

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Mearthane Products Corporation (MPC)
Trade Name Durethane™ F
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mearthane Durethaneâ„¢ F DF-245A Closed Cell Foam Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TDI backbone: ester.Shore 00 Hardness: 90Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient of friction, abrasion resistance, hardness and density) to suit various application. The rebound can be formulated for resiliency or energy absorption.Applications: Applications for Durethane F include self-cleaning paper feed rollers, retard pads, conveyor belts, bumpers shock absorbers and timing belts.Conductivity: All Durethane elastomers can be formulated to be electrically conductive, for applications involving electrostatic dissipation (ESD). Mearthane's proprietary conductivity process does not comprise the material performance specification of the urethane.Information provided by Mearthane Products Corporation.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D3574A
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
ASTM D2240
Tensile Strength, Ultimate 69.0 MPa
10000 psi
ASTM D3574E
Elongation at Break 400 %
400 %
ASTM 3457E
100% Modulus 0.00110 GPa
0.160 ksi
Compressive Yield Strength 0.540 MPa
78.3 psi
at 10% deflection; ASTM D3574C
0.600 MPa
87.0 psi
at 20% deflection; ASTM D3574C
1.02 MPa
148 psi
at 30% deflection; ASTM D3574C
Resilience 36
36
Bashore Rebound; ASTM 2632D
Tear Strength Test 137
137
lb; Die C; ASTM 3457F