Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) 5218EA High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) 5218EA High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HD-5218EA is a high density polyethylene copolymers containing butane-1 as the comonomer with narrow molecular weight distribution, suitable for thin wall injection application. It has been designed for fast cycling application and low warpage with a good balance of toughness and stiffness characteristics. Applications: houseware, thin walled containers, food container, toys, home utensil.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D1505
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 190 °C
18 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
52 g/10 min

@Load 5.00 kg,
Temperature 190 °C
52 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 900 %
900 %
ASTM D638
Flexural Modulus 1.05 GPa
152 ksi
ASTM D790
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 115 °C
239 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 131 °C
268 °F
180 - 250 °C
356 - 482 °F