Polymer Property : Film Tensile Strength at Yield, MD = 12.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO 527-3
Polimeri Europa Clearflex® FG 306 Hexene Copolymer Linear Low Density Polyethylene
Clearflex FG 306 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, antiblocking and processing aid, suitable for blown film extrusion.Films manufactured with Clearf..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ASTM D882
SABIC 218 Series Linear Low Density Polyethylene for Blown Film
Product Description: 218 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. They are easy to process giving good tensile properties, impact strength a..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ASTM D882
SABIC 218B Linear Low Density Polyethylene for Cast Film
Product Description: 218B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ASTM D882
SABIC 6821N Linear Low Density Polyethylene for Blown Film
Product Description: 6821N is a fractional melt index hexene copolymer based Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resi..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO 527-3
Polimeri Europa Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 30 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 are characterized by an..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO 527-3
Polimeri Europa Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 30 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 U are characterized b..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ASTM D882
Reliance Industries Reclair F22020 Polyethylene
Butene comonomer based Linear Low Density Polyethylene blow film grade. Reclair F22020 has optimum levels of antioxidants, antiblocking agents, and slip additives. Applications:general purpose, and..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO 527-3
Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion
Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
2 in per min; ASTM D882
Chevron Phillips mPact™ D353 m-MDPE Linear Low Density Polyethylene  (discontinued **)
Low Density PolyethyleneCustomer Benefits: This metallocene medium density PE for cast film applications offers greater tensile modulus than LLDPE while retaining excellent optical properties.Data p..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ASTM D882
ExxonMobil Escorene® LL-1117 LLDPE Film/Sandwich Bag Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin. Films made from LL-1117 have very good tensile properties and toughness. This resin's good strength and drawability all..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ASTM D882
Iran Petrochemical (PCC) Arak 0410AA LLDPE  (discontinued **)
Information provided by Iran Petrochemical Commercial Co.
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ASTM D882
Westlake Hifor SC74561-F Clear (Voridian) Polyethylene Film, Using Energx Technology Services  (discontinued *
VORIDIAN HIFOR CLEAR SC74558-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives. Films produced with t..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ASTM D882
ExxonMobil Escorene® LD-108 LDPE Packaging Film Resin, High Clarity  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer high clarity film resin with a good balance of toughness, stiffness, and drawdown capability. This resin has good machinability in ba..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ASTM D882
ExxonMobil Escorene® LD-140 LDPE Industrial Film resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A fractional melt index homopolymer resin for production of film with very good toughness.Applications: Heavy duty bags. Data for film properties b..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ASTM D882-02
Ipiranga Petrochem LBH 0120 BPS LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO R527-1
Iran Petrochemical (PCC) 2101TN47 Low Density Polyethylene
LDPE 2101TN47 Shrink FilmThis grade enables high speed production of film without blocking.Information provided by Iran Petrochemical Commercial Co.
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO R527-1
Iran Petrochemical (PCC) 2501TN00 Low Density Polyethylene
LDPE 2501TN00 Hygienic Film It is used in diaper film, lamination film and in applications where low blocking behavior without the help of additives is required.Information provided by Iran Petroch..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ASTM D882-02
Ipiranga Petrochem LBH 0120 BP LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO R527-1
Iran Petrochemical (PCC) 2004TC37 Low Density Polyethylene
LDPE 2004TC37: Light duty film used for very thin films requiring good optical properties for general packaging.Information provided by Iran Petrochemical Commercial Co.
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ASTM D882
Iran Petrochemical (PCC) 235F7 Linear Low Density Polyethylene
235F7 is a LLDPE blown film grade designed for general purpose film application. This resin is particularly suited for blending with LDPE, giving better strength and downgauging possibility.Informat..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO 527
Iran Petrochemical (PCC) LT0470/KJ Low Density Polyethylene
LT0470/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. Application: stiffer thin films for textile p..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ASTM D882
SCG Chemicals EL-Leneâ„¢ L2009FA Linear Low Density Polyethylene Film
Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains no slip agent and antiblocking agentRecommended App..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO 527-3
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film
LDPE 1022 FH 24 is a low density polyethylene made by a high pressure process.LDPE 1022 FH 24 is a slip and anti-block formulated grade.LDPE 1022 FH 24 is suited to many applications in the field of..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
Dow DOWLEX™ 2070D Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2070D Polyethylene resin is a fully formulated linear low density polyethylene resin offering high strength and low gel properties for blown film food packaging applications. DOWLEX 2070D r..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
Dow LDPE 494A Low Density Polyethylene, Film Grade
DOW LDPE 494A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 494A resin can be blended with most linear low density..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ASTM D882
Iran Petrochemical (PCC) Arak 0640AA LLDPE  (discontinued **)
Information provided by Iran Petrochemical Commercial Co.
Film Tensile Strength at Yield, MD >= 12.0 MPa
>= 1740 psi
Iran Petrochemical (PCC) Tabriz 0410AA LLDPE  (discontinued **)
Information provided by Iran Petrochemical Commercial Co.
Film Tensile Strength at Yield, MD 12.0 - 30.0 MPa
1740 - 4350 psi
Average value: 24.2 MPa Grade Count:5
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO 527-3
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film
LDPE 1022 FN 24 is a low density polyethylene made by a high pressure process without antioxidant.LDPE 1022 FN 24 is suited to many applications in the field of consumer, industrial, food or hygiene..