Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 30.0 kN/m | 171 pli | ISO 34-1 |
PolyOne OnFlex™ S FR 70A-3S1890 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Tear Strength | >= 30.0 kN/m | >= 171 pli | DIN 53507 |
Karina TR-605-22/23 Crepe PVC Compound PVC compound additivated with nitrile rubber.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 30.0 kN/m | 171 pli | TD; ISO 6383-2 |
Iran Petrochemical (PCC) 2101TN47 Low Density Polyethylene LDPE 2101TN47 Shrink FilmThis grade enables high speed production of film without blocking.Information provided by Iran Petrochemical Commercial Co. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2631 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2670 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2750 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 4640 FC Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Die B |
Momentive Performance Materials Silplusâ„¢ 30 HS High Strength Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | TD; ISO 6383-2 |
Iran Petrochemical (PCC) 2004TC37 Low Density Polyethylene LDPE 2004TC37: Light duty film used for very thin films requiring good optical properties for general packaging.Information provided by Iran Petrochemical Commercial Co. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Die B |
Momentive Performance Materials Addisilâ„¢ 480 E Healthcare Extrusion Grade Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3386/40 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
Shin-Etsu Silicones LIMSâ„¢ KE2095-50AB Elastomer KE-2095-50 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
Trelleborg R399 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
Trelleborg R439 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
Trelleborg R570 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
Trelleborg T621 Butyl Rubber Butyl rubber is a copolymer of isobutylene and a small percentage of isoprene.PropertiesWith careful compounding Butyl has really good tensile strength.Butyl has very low permeability to air and oth.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
Trelleborg B739 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
Trelleborg R504 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 30.0 kN/m | 171 pli | ASTM D624 |
ELASTO UK Dryflex® 602600S SEBS Based Material, Filled Qualities, 60A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 30.0 kN/m | 171 pli | ASTM D624 |
ELASTO UK Dryflex® 602650S SEBS Based Material, Filled Qualities, 65A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® F 47 H NL nat 6020 PA6 Product description: Grilon F 47 HNL natural 6020 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good mechanical propertiesGood barrier against oils and fa.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® F 40 NL PA6 Product description: Grilon F 40 NL natural 6018 is a nucleated and lubricated high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGoo.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® F 47 NL nat 6028 PA6 Product description: Grilon F 47 NL natural 6028 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGood barrier agai.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | |
ACC MM940 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | ISO 34-B |
AlphaGary Evoprene™ Super G 931 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | ISO 34-B |
AlphaGary Evoprene™ G 991 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Tear Strength | 30.0 kN/m | 171 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® F 50 nat 6368 PA6 Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes: Very high melt strengthGood chemical resistanceGood gas-barrierGood mechanical pro.. |