Multibase Multi-Flex® TPO D-6208

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO D-6208.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792-91
Melt Flow 7.0 g/10 min
7.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
10 sec; ASTM D-2240-95
Flexural Modulus 0.998 GPa
145 ksi
Method 1, Proc. B; ASTM D-790-95
Tear Strength 61.0 kN/m
348 pli
ASTM D624-95