Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 200 J/cm | 375 ft-lb/in | ASTM D4272 |
Iran Petrochemical (PCC) 2501TN00 Low Density Polyethylene LDPE 2501TN00 Hygienic Film It is used in diaper film, lamination film and in applications where low blocking behavior without the help of additives is required.Information provided by Iran Petroch.. |
|||
Tensile Impact | 200 J/cm | 375 ft-lb/in | ASTM D4272 |
Iran Petrochemical (PCC) LF0190 Low Density Polyethylene LF01090 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: general pupose film and for aminati.. |
|||
Tensile Impact | 200 J/cm | 375 ft-lb/in | ASTM D4272 |
Iran Petrochemical (PCC) LF0250/KJ Low Density Polyethylene LF0250/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: packaging films.Information provid.. |
|||
Tensile Impact | 200 J/cm | 375 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 2523 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 200 J/cm | 375 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 7562 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |