Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene Clearflex FG 308 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 308 ar.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 336 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, slip agent, antiblocking agent and processing aid, suitable for blown film extrusion.Films obtain.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
SABIC 218 Series Linear Low Density Polyethylene for Blown Film Product Description: 218 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. They are easy to process giving good tensile properties, impact strength a.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
SABIC 218B Linear Low Density Polyethylene for Cast Film Product Description: 218B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
SABIC 6821N Linear Low Density Polyethylene for Blown Film Product Description: 6821N is a fractional melt index hexene copolymer based Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resi.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 30 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 U are characterized b.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion Riblene FC 40 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 40 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
Reliance Industries Reclair F22020 Polyethylene Butene comonomer based Linear Low Density Polyethylene blow film grade. Reclair F22020 has optimum levels of antioxidants, antiblocking agents, and slip additives. Applications:general purpose, and.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | 2 in per min; ASTM D882 |
Chevron Phillips mPact™ D353 m-MDPE Linear Low Density Polyethylene
(discontinued **) Low Density PolyethyleneCustomer Benefits: This metallocene medium density PE for cast film applications offers greater tensile modulus than LLDPE while retaining excellent optical properties.Data p.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
Iran Petrochemical (PCC) Arak 0410AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
Westlake Hifor SC74561-F Clear (Voridian) Polyethylene Film, Using Energx Technology Services
(discontinued * VORIDIAN HIFOR CLEAR SC74558-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives. Films produced with t.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
ExxonMobil Escorene® LD-108 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer high clarity film resin with a good balance of toughness, stiffness, and drawdown capability. This resin has good machinability in ba.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
ExxonMobil Escorene® LD-140 LDPE Industrial Film resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index homopolymer resin for production of film with very good toughness.Applications: Heavy duty bags. Data for film properties b.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO R527-1 |
Iran Petrochemical (PCC) 2101TN47 Low Density Polyethylene LDPE 2101TN47 Shrink FilmThis grade enables high speed production of film without blocking.Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO R527-1 |
Iran Petrochemical (PCC) 2501TN00 Low Density Polyethylene LDPE 2501TN00 Hygienic Film It is used in diaper film, lamination film and in applications where low blocking behavior without the help of additives is required.Information provided by Iran Petroch.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882-02 |
Ipiranga Petrochem LBH 0120 BP LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527 |
Iran Petrochemical (PCC) LS0085/KJ Low Density Polyethylene LS0085/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: shrink packaging.Information prov.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527 |
Iran Petrochemical (PCC) LT0470/KJ Low Density Polyethylene LT0470/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. Application: stiffer thin films for textile p.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ L2009F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ L2009FA Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains no slip agent and antiblocking agentRecommended App.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | |
Westlake Hifor SC74557 Linear Low Density Polyethylene WESTLAKE Hifor Clear Polyethylene SC74557 is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and low antiblock. Films produc.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film LDPE 1022 FH 24 is a low density polyethylene made by a high pressure process.LDPE 1022 FH 24 is a slip and anti-block formulated grade.LDPE 1022 FH 24 is suited to many applications in the field of.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | |
Dow LDPE 494A Low Density Polyethylene, Film Grade DOW LDPE 494A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 494A resin can be blended with most linear low density.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ASTM D882 |
Iran Petrochemical (PCC) Arak 0640AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, MD | >= 12.0 MPa | >= 1740 psi | |
Iran Petrochemical (PCC) Tabriz 0410AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 1184 |
Iran Petrochemical (PCC) Tabriz 0640AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, MD | 12.0 - 30.0 MPa | 1740 - 4350 psi | Average value: 24.2 MPa Grade Count:5 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film LDPE 1022 FN 24 is a low density polyethylene made by a high pressure process without antioxidant.LDPE 1022 FN 24 is suited to many applications in the field of consumer, industrial, food or hygiene.. |
|||
Film Tensile Strength at Yield, MD | 12.0 MPa | 1740 psi | ISO 527-3 |
Total Lumicene® mPE M 3427 Metallocene Polyethylene, Cast Film Lumicene® mPE M 3427 is a second generation metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 3427 can be processed at high output rates with low extrusion pressure, low neck.. |