Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene Clearflex FG 308 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 308 ar.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Clearflex® FG 368 Octene Comonomer Linear Low Density Polyethylene Clearflex FG 368 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 368 ar.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
SABIC 726 Series Linear Low Density Polyethylene for Blown Film Product Description: 726 series resins are fractional index Linear Low Density Polyethylene grades suitable for blown film applications. Films produced using these resins give a relatively higher .. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion Riblene FC 40 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 40 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Riblene® FM 34 Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 is characterized by a good balance between processabilit.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
NOVA Chemicals Novapol® 20% LF-0718-A in PF-0118-B LDPE Film Resin Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical .. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
NOVA Chemicals Novapol® 5% LF-0718-A in PF-0118-B LDPE Film Resin Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical .. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0224-A LDPE Foam Resin Excellent stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
Reliance Industries Reclair F18010 Polyethylene Butene comonomer based Linear Low Density Polyethylene blow film grade. Applications:lamination films. Information provided by Reliance Industries |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ISO 527-3 |
Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
NOVA Chemicals Sclair® 11U4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, easy processability.Applications: Bread bags, HDPE bottle sleeves, specialty blending.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0224-A LDPE
(discontinued **) Puncture value is 43.2 J/mm. LDPE. Excellent stiffness, moderate toughness, easy processability. Additive Package: Base Resin.Applications: Industrial packaging, liners, blends with LLDPE, foam art.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
ExxonMobil Escorene® LD-103 LDPE Industrial Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer industrial film resin with excellent toughness. LD-103 has a low melt index which gives excellent impact strength and melt strength o.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
ExxonMobil Escorene® LD-108 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer high clarity film resin with a good balance of toughness, stiffness, and drawdown capability. This resin has good machinability in ba.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
ExxonMobil Escorene® LD-138 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin offering good clarity, toughness, and stiffness. Blown film made from this resin has good machinability in bag equipment a.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
Reliance Industries Reclair F18020 Polyethylene Butene comonomer based Linear Low Density Polyethylene cast film grade. Reclair F18020 has optimum levels of antioxidants, and polymer processing aids. Applications:cast films, air bubble films, an.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
Reliance Industries Reclair F19010 Polyethylene Blow film Linear Low Density Polyethylene grade. Reclair F19010 is butene comonomer based, with optimum levels of antioxidants, antiblocking agents, slip additives, and polymer processing aids. Th.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882-02 |
Ipiranga Petrochem LB 0120 BPS LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882-02 |
Ipiranga Petrochem LBH 0117 LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ISO R527-1 |
Iran Petrochemical (PCC) 2501TN00 Low Density Polyethylene LDPE 2501TN00 Hygienic Film It is used in diaper film, lamination film and in applications where low blocking behavior without the help of additives is required.Information provided by Iran Petroch.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882-02 |
Ipiranga Petrochem LBH 0120 BP LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ISO 527 |
Iran Petrochemical (PCC) LT0470/KJ Low Density Polyethylene LT0470/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. Application: stiffer thin films for textile p.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ LD1902F Low Density Polyethylene Film Key Characteristics:High strengthGood optical propertiesCan be blended with HDPE, LLDPESafe for food contactContains 1400 ppm slip content and 2400 ppm antiblocking contentRecommended Applications:G.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ LD1902FA Low Density Polyethylene Film Key Characteristics:High strengthGood optical propertiesCan be blended with HDPE, LLDPESafe for food contactRecommended Applications:General purpose bag, big bagMedium-weight shrink filmInformation .. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ISO 527-3 |
Total Lumicene® mPE M 2310 EP Metallocene Polyethylene, Blown Film Lumicene® mPE M 2310 EP is a second generation metallocene based Linear Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2310 EP can be processed at high output rates with low ext.. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ASTM D882 |
Iran Petrochemical (PCC) Arak 0640AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Yield, TD | 12.0 MPa | 1740 psi | ISO 1184 |
Iran Petrochemical (PCC) Tabriz 0640AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |