Material Notes:
High heat, high molecular weight general purpose polystyrene with low crystal clarity. It offers high stiffness for extrusion/thermoforming applications, especially for the food packaging.Information provided by BASF.Ineos Styrenics purchased this product line from BASF in 2005.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Flow 1.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 78
78
ASTM D785
Tensile Strength, Ultimate 52.0 MPa
7540 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 2.55 GPa
370 ksi
ASTM D638
Flexural Modulus 3.31 GPa
480 ksi
ASTM D790-1
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C
201 °F
ASTM D648
Vicat Softening Point 109 °C
228 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Processing Properties Metric English Comments
Melt Temperature 210 - 240 °C
410 - 464 °F
Molding Temp