Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.31 GPa | 480 ksi | |
Quadrant EPP Ertalon® 6XAU+ PA 6, heat stabilized, cast (ISO Data) Ertalon 6 XAU+ is a heat stabilized cast nylon grade with a very dense and highly crystalline structure. Compared with conventional extruded or cast nylons, Ertalon 6 XAU+ offers superior heat agein.. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Quantum Nylon 6/6 MoS2 Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
I. Stern WC-102 General Purpose Crystal Polystyrene Features:Good Processing CharacteristicsUL Classification 94 HBExcellent Water ClarityComplies with FDA Title 21 CFR 177.1640ApplicationsExtrusion FoamDisplaysInformation provided by I. Stern & Co. .. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Global GPC-110 10% Glass Reinforced Polycarbonate Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Global GPC-FR-510 10% Glass Filled Flame Resistant Polycarbonate Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790-1 |
Ineos Styrenics Polystyrene 168M (NAFTA) High heat, high molecular weight general purpose polystyrene with low crystal clarity. It offers high stiffness for extrusion/thermoforming applications, especially for the food packaging.Informati.. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer LNP THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing 20% Milled Glass. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer (Asia Pacific) LNP* THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D 790 |
Styrolution PS 1290/1291 GPPS Extrusion / thermoforming foam sheetLow residual styrene monomer contentHigh melt strength and stiffnessUL Classification 94 HB for 1290Information provided by Styrolution |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D 790 |
Styrolution PS 1300/1301 GPPS Profile extrusionGood balance of flow and strengthHigh stiffnessUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D 790 |
Styrolution PS 1600 GPPS Foam extrusion; Injection moldingGood balanced of strength, flow and heat resistanceFree of zinc and oil additivesInformation provided by Styrolution |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D 790 |
Styrolution PS 1611 GPPS Injection moldingGood balance of flow, strength and set-up propertiesUL Classification 94 HBInformation provided by Styrolution |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D 790 |
Styrolution PS 3600/3601 GPPS Exceptional flow characteristicsGood for thin wall and complex partsUSP Class VI certifiedInformation provided by Styrolution |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Techmer ES Electrablend® ABS 03011 BK MB Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Conductive, Electromagnetic Shielding (EMI) and Radio Frequency Shielding (RFI)Appearance: BlackIn.. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFLAM™ FPP 1007F Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007F is a 40% talc filled homopolymer polypropylene compound that utilizes FDA compliant raw materials.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFLAM™ FPP 1007F Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007F is a 40% talc filled homopolymer polypropylene compound that utilizes FDA compliant raw materials.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Total PSC 523 Polystyrene Polystyrene 523 is a high flow, high heat crystal. Specially designed for foam applications it has a very narrow molecular weight distribution. Performance in extruded loose fill foam is excellent d.. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Entec Hyrene® PSCRY 14 General Purpose Polystyrene Available in North America Features: General PurposeRoHS Compliant Form: Pellets Information provided by Entec |
|||
Flexural Modulus | 3.31 GPa | 480 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp TX88477 PU LNP* Thermocomp* TX88447 is a compound based on Polyurethane resin containing proprietary fillers.This data was supplied by SABIC-IP for the Americas region. |