Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42

Category Metal , Ferrous Metal , Austenitic , Stainless Steel , T S30000 Series Stainless Steel
Manufacturer Groupe Arcelor
Trade Name URANUS®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: URANUS® B25 (UR B25) is a 18% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed to be cost effective. The 18% nickel and 0.7% copper additions combined with the chromium and molybdenum additions improve the behavior of the steel in many corrosive solutions encountered for example in chemical and petrochemical processes or chloride containing solutions. The alloy is also seawater resistant and has extensively been used in offshore industries (It has not to be used in stagnant seawater application with temperatures higher than 30° 86°F). Thanks to the 18% Nickel and the 0.2 Nitrogen additions, the microstructure is austenitic.Information provided by manufacturer.
Physical Properties Metric English Comments
Density 8.00 g/cc
0.289 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 190 - 230
190 - 230
Typical, V<sub>10</sub>
Tensile Strength, Ultimate >= 650 MPa
>= 94300 psi
Minimum Guaranteed
Tensile Strength, Yield >= 300 MPa

@Strain 0.200 %
>= 43500 psi

@Strain 0.200 %
>= 330 MPa

@Strain 1.00 %
>= 47900 psi

@Strain 1.00 %
Elongation at Break >= 35 %
>= 35 %
Modulus of Elasticity 195 GPa
28300 ksi
Poissons Ratio 0.30
0.30
Calculated
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Charpy Impact >= 60.0 J

@Temperature -196 °C
>= 44.3 ft-lb

@Temperature -321 °F
Thermal Properties Metric English Comments
CTE, linear 16.5 µm/m-°C

@Temperature 20.0 - 100 °C
9.17 µin/in-°F

@Temperature 68.0 - 212 °F
17.0 µm/m-°C

@Temperature 20.0 - 300 °C
9.44 µin/in-°F

@Temperature 68.0 - 572 °F
17.3 µm/m-°C

@Temperature 20.0 - 500 °C
9.61 µin/in-°F

@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.480 J/g-°C

@Temperature 20.0 °C
0.115 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 13.0 W/m-K

@Temperature 20.0 °C
90.2 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Carbon, C 0.010 %
0.010 %
Chromium, Cr 20 %
20 %
Copper, Cu 0.70 %
0.70 %
Iron, Fe 54.989 %
54.989 %
As remainder
Molybdenum, Mo 6.1 %
6.1 %
Nickel, Ni 18 %
18 %
Nitrogen, N 0.20 %
0.20 %
Sulfur, S 0.0010 %
0.0010 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000900 ohm-cm

@Temperature 20.0 °C
0.0000900 ohm-cm

@Temperature 68.0 °F
Users viewing this material also viewed the following: