Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 650 MPa | 94300 psi | Outokumpu Typical, Annealed Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4021 Martensitic Stainless Steel Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat.. |
|||
Tensile Strength, Ultimate | >= 650 MPa | >= 94300 psi | |
Kobe Steel KS100 Commercially Pure Titanium, Annealed Nominal Composition: Ti-Fe-OApplications: Wrist watches, cutlery, golf club heads.Features: Scratch resistant, easy to polish, high strength. Information provided by Kobe Steel |
|||
Tensile Strength, Ultimate | >= 650 MPa | >= 94300 psi | Minimum Guaranteed |
Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42 Description: URANUS® B25 (UR B25) is a 18% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed to be cost effective. The 18% nickel and 0... |
|||
Tensile Strength, Ultimate | >= 650 MPa | >= 94300 psi | Minimum Guaranteed |
Industeel URANUS® B26 6 Mo High Performance Super-Austenitic Stainless Steel with PREN = 43 Description: URANUS® B26 (UR B26) is a 25% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed for high structural stability and high corr.. |
|||
Tensile Strength, Ultimate | 650 MPa @Temperature 760 °C |
94300 psi @Temperature 1400 °F |
|
Haynes 188 alloy, hot rolled and 1175°C solution annealed plate Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Ultimate | 650 MPa | 94300 psi | Annealed |
Special Metals INCOLOY® Alloy MA 956 An iron-chromium-aluminum alloy that is oxide dispersion strengthened and produced by mechanical alloying. Production involves high-energy milling of metal powders to create an alloy with a strengt.. |
|||
Tensile Strength, Ultimate | >= 650 MPa | >= 94300 psi | |
SSAB Tunnplat Domex® 590XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Tensile Strength, Ultimate | 650 - 820 MPa | 94300 - 119000 psi | |
SSAB Tunnplat Domex® 600MC HSLA Steel HSLA SteelCharacteristics: Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better properties.Property data is for hot-rolled steel..Domex® is the brand n.. |
|||
Tensile Strength, Ultimate | 650 MPa | 94300 psi | Typical |
TIMET TIMETAL® 3-2.5 -0.05Pd Titanium Alloy Cold Workable Medium Strength Alloy. Palladium is added to this grade to enhance its corrosion behavior. Property data below is typical of TIMETAL® 3-2.5 Titanium Alloy.Data provided by TIMET. |
|||
Tensile Strength, Ultimate | 650 MPa | 94300 psi | Typical |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Typical Properties Cold Workable Medium Strength AlloyFeatures: Cold formable and weldable, this alloy is used primarily for honeycomb foil and hydraulic tubing applications. Industrial applications such as pressure v.. |
|||
Tensile Strength, Ultimate | 650 - 800 MPa | 94300 - 116000 psi | Rod |
CLAL-MSX ARCAP Anticorrosion AP4 H14 4/4 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Tensile Strength, Ultimate | 650 - 850 MPa | 94300 - 123000 psi | |
CLAL-MSX NICLAL 1800 H14 4/4 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good corrosion resistanceHigh mechanical propertiesTypical Applications:Parts subject to high stressHigh quality fastenersInformation provided by CLAL-MSX |
|||
Tensile Strength, Ultimate | >= 650 MPa | >= 94300 psi | Wire |
CLAL-MSX ARCAP Anticorrosion AP1 H15 Spring, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Tensile Strength, Ultimate | 650 - 750 MPa | 94300 - 109000 psi | Wire |
CLAL-MSX ARCAP Anticorrosion AP1C H12 1/2 hard, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Tensile Strength, Ultimate | 650 - 750 MPa | 94300 - 109000 psi | Wire |
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Tensile Strength, Ultimate | 650 - 730 MPa | 94300 - 106000 psi | |
ArcelorMittal HSLA 550 High strength low alloy steel for cold forming, Hot Rolled Available in the following: S550MCDescription: Steels in the HSLA (High Strength Low Alloy) range are hardened by a combination of precipitation and grain size refining, resulting in high strength w.. |
|||
Tensile Strength, Ultimate | 650 MPa | 94300 psi | Transverse |
AK Steel ULTRALUME® Press Hardenable Carbon Steel ULTRALUME Press Hardenable Steel (PHS) is AK Steel’s newest addition to our expanding product portfolio of Advanced High Strength Steels (AHSS). Aluminized Type 1 ULTRALUME PHS is intended for auto.. |
|||
Tensile Strength, Ultimate | 650 - 850 MPa | 94300 - 123000 psi | Minimum Guaranteed |
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT650 Heat Treatment) Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g.. |