Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.00 g/cc | 0.289 lb/in³ | ISO 1183 |
PolyOne Trilliant™ HC HC0200-5001 XR Grey Thermoplastic Elastomer (TPE) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | theoretical |
Kennametal Stellite Deloro® 711 PM after P/M Processing Deloro 711 is currently being developed. Adhesive wear test data: P/M 0.1, cast 0.1; Abrasive wear test data P/M 6 mm^3, cast 26 mm^3. Typical applications include vane plugs, fuel metering pins, sp.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Industeel URANUS® B28 High Nickel Super-Austenitic Stainless Steel Description: URANUS® B28 (UR B28) is a super-austenitic stainless steel with very high nickel (31%) and chromium (27%) contents. The molybdenum content is about 3.5%. The alloy is designed for sp.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Lucas-Milhaupt FOS FLO 7 Copper Phosphorus Alloy Applications:Fos-Flo 7 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in service.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Lucas-Milhaupt SIL-FOS 2 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 2 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in servi.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Indium Corp. Indalloy 110 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Industeel SIRIUS 800 Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at t.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
ATI Allegheny Ludlum AL 4565™ Corrosion Resistant Stainless Steel Characteristics:Very high resistance to pitting and crevice corrosion Excellent general corrosion resistance in a variety of media Higher mechanical propertied then conventional stainless steels Go.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Industeel SIRIUS 800 H Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at tempe.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 904L High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |