Mechanical Properties Metric English Comments
Shear Modulus 75.0 GPa
10900 ksi
calculated
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel NUCL 18.10 B4 Natural Boron (Min 1% wt) Alloyed 304 Stainless Steel
Description: Isotope B10 has the property to capture neutrons produced by nuclear reactions. Natural boron contains about 19.9 at% or 18.45 wt % of B10 isotope, the remaining being B11 isotope. NUCL..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel SIRIUS 309 23% Cr - 13% Ni Heat Resistant Stainless Steel
Description: CLI SIRIUS 309 grade is a fully austenitic stainless steel containing 23% Cr, and 13% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resistance b..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel
Description: CLI SIRIUS 310 grade is a fully austenitic stainless steel containing 25% Cr, 0.6% Si and 20% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resi..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel SIRIUS 314 25% Cr - 1.8% Si Heat Resistant Stainless Steel
Description: CLI SIRIUS 314 grade is a fully austenitic stainless steel containing 25% Cr, 20% Ni and 1.8% Si. The alloy is designed for high temperature corrosion resistance applications even in se..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel SIRIUS S12 20% Cr - 1.8% Si Heat Resistant Steel
Description: CLI SIRIUS S12 grade is an austenitic stainless steel containing 20% Cr, 1.8 % Si and 12% Ni. The low nickel content combined with high chromium and high silicon contents provide good r..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel SIRIUS S15 Rare Earth Containing Heat Resistant Steel
CLI SIRIUS S15 grade is a fully austenitic stainless steel containing 21 Cr, 1.7 Si, 0.17 N and Rare Earth elements (Cerium, Lanthanum,...etc) which make the alloy particularly well designed for hig..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24
Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its me..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to re..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel URANUS® 65 310 L Modified Grade - Low C and Si for Nitric Acid Service
Description: URANUS® 65 is a 25 Cr 20 Ni austenitic stainless steel with sharp control of the residual elements in order to provide high corrosion resistance properties in boiling 50-65% Nitric a..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42
Description: URANUS® B25 (UR B25) is a 18% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed to be cost effective. The 18% nickel and 0...
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel URANUS® B26 6 Mo High Performance Super-Austenitic Stainless Steel with PREN = 43
Description: URANUS® B26 (UR B26) is a 25% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed for high structural stability and high corr..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel URANUS® B28 High Nickel Super-Austenitic Stainless Steel
Description: URANUS® B28 (UR B28) is a super-austenitic stainless steel with very high nickel (31%) and chromium (27%) contents. The molybdenum content is about 3.5%. The alloy is designed for sp..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel URANUS® B6 Multipurpose Austenitic Stainless Steel with PREN = 34
Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel URANUS® B6 N Multipurpose Austenitic Stainless Steel with PREN = 36
Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel URANUS® B66 High Strength Super-Austenitic Stainless Steel with PREN = 54
Description: Research carried out these last five years has shown that combined additions of chromium, tungsten, molybdenum, nitrogen and copper, make it possible to design a super-austenitic stainl..
Shear Modulus 75.0 GPa

@Temperature 371 °C
10900 ksi

@Temperature 700 °F
Haynes R-41 alloy, 0.635 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Shear Modulus 75.0 GPa

@Temperature 371 °C
10900 ksi

@Temperature 700 °F
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Shear Modulus 75.0 GPa

@Temperature 371 °C
10900 ksi

@Temperature 700 °F
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F)
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red..
Shear Modulus 75.0 GPa
10900 ksi
Elgiloy® Co-Cr-Ni Alloy, Wire, 20% Cold Reduction
The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f..
Shear Modulus 75.2 GPa
10900 ksi
Carlson C 200 Commercially Pure Nickel
General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at..
Shear Modulus 75.2 GPa
10900 ksi
Carlson C 201 Commercially Pure Nickel
General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34
Description: URANUS® 45N (UR 45N) is a nitrogen alloyed (= 0.15%) austenitic-ferritic stainless steel (22.05 type) with improved structure stability and high general, localized and stress corrosion..
Shear Modulus 75.0 GPa
10900 ksi
calculated
Outokumpu 904L High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel
Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chrom..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel UREA 25.22.2 Plants
Description: CLI UREA 25.22.2 chemical composition has been optimized for specific uses in Urea plants. It is a 310L modified austenitic stainless steel with low carbon, low silicon and high nitroge..
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Industeel UREA 316L Modified 316L Mod Low Si, High Mo Stainless Steel for Urea Plants
Description: UREA 316L Modified grade has been specially developed for Urea plant applications. It is a 316L modified stainless steel with extra-low silicon content and substantial higher molybdenum..